HMC Electronics 38050 Loctite 380 Black Max Tough Instant Adhesive User Manual

Loctite

Advertising
background image

Technical Data Sheet

LOCTITE

®

380

May

-

2004

PRODUCT DESCRIPTION
LOCTITE

®

380 provides the following product characteristics:

Technology

Cyanoacrylate

Chemical Type

Ethyl cyanoacrylate

Appearance (uncured)

Black liquid

LMS

Components

One part - requires no mixing

Viscosity

Medium

Cure

Humidity

Application

Bonding

Key Substrates

Metals, Plastics and Rubbers

LOCTITE

®

380 is a rubber toughened adhesive with increased

flexibility and peel strength along with enhanced resistance to
shock.

TYPICAL PROPERTIES OF UNCURED MATERIAL

Specific Gravity @ 25 °C

1.1

Viscosity, Brookfield - RVT, 25 °C, mPa·s (cP):

Spindle 3, speed 50 rpm

100 to 800

LMS

Flash Point - See MSDS

TYPICAL CURING PERFORMANCE

Under normal conditions, the atmospheric moisture initiates the

curing process. Although full functional strength is developed

in a relatively short time, curing continues for at least 24 hours

before full chemical/solvent resistance is developed.

Cure Speed vs. Substrate

The rate of cure will depend on the substrate used. The table

below shows the fixture time achieved on different materials

at 22 °C / 50 % relative humidity. This is defined as the time to

develop a shear strength of 0.1 N/mm².

Fixture Time, ISO 4587, seconds:

Steel (degreased)

60 to 120

Aluminum

10 to 30

Neoprene

15 to 25

Rubber, nitrile

15 to 25

ABS

20 to 50

PVC

50 to 100

Polycarbonate

30 to 90

Phenolic

20 to 60

Cure Speed vs. Bond Gap

The rate of cure will depend on the bondline gap. Thin bond

lines result in high cure speeds, increasing the bond gap will

decrease the rate of cure.

Cure Speed vs. Activator

Where cure speed is unacceptably long due to large gaps,

applying activator to the surface will improve cure speed.

However, this can reduce ultimate strength of the bond and

therefore testing is recommended to confirm effect.

TYPICAL PROPERTIES OF CURED MATERIAL

After 24 hours @ 22 °C

Physical Properties:

Coefficient of Thermal Expansion, ASTM D 696, K

-1

80×10

-6

Coefficient of Thermal Conductivity, ASTM C 177,

W/(m·K)

0.1

Glass Transition Temperature, ASTM E 228, °C

120

Electrical Properties:

Dielectric Constant / Dissipation Factor, ASTM D 150:

0.05

-

kHz

2.65 / <0.02

1

-

kHz

2.75 / <0.02

1,000

-

kHz

2.75 / <0.02

Volume Resistivity, ASTM D 257, Ω·cm

10×10

15

Dielectric Breakdown Strength, ASTM D 149, kV/mm

25

TYPICAL PERFORMANCE OF CURED MATERIAL

Adhesive Properties

After 24 hours @ 22 °C

Lap Shear Strength, ISO 4587:

Steel (grit blasted)

N/mm² 26

(psi) (3,770)

Aluminum (etched)

N/mm² 18

(psi) (2,610)

ABS

N/mm² >6

(psi) (>870)

PVC

N/mm² >4

(psi) (>580)

Polycarbonate

N/mm² >5

(psi) (>725)

Phenolic

N/mm² 10

(psi) (1,450)

Neoprene

N/mm² >10

(psi) (>1,450)

Nitrile

N/mm² >10

(psi) (>1,450)

Tensile Strength, ISO 6922:

Steel (grit blasted)

N/mm² 18.5

(psi) (2,700)

After 48 hours @ 22 °C

Lap Shear Strength, ISO 4587:

Steel (grit blasted)

N/mm² ≥17.2

LMS

(psi) (≥2,495)

Cured for 24 hours @ 22 °C, followed by 24 hours @ 121 °C,

tested @ 121 °C

Lap Shear Strength, ISO 4587:

Steel (grit blasted)

N/mm² ≥6.9

LMS

(psi) (≥1,000)

Cured for 24 hours @ 22 °C, followed by 24 hours @ 121 °C,

tested @ 22 °C

Lap Shear Strength, ISO 4587:

Steel (grit blasted)

N/mm² ≥19.3

LMS

(psi) (≥2,800)

Documentation Provided By HMC Electronics