a. The printer supports a wide range of media sizes.
b. Capacity may vary depending on print materials weight and thickness, as well as environmental conditions.

 

Guidelines for Using Paper

 

For best results, use conventional 75 g/m

2

(20 lb) paper. Ensure the paper is of good quality, free of cuts, nicks, tears, spots, loose particles, dust, wrinkles,

voids, and curled or bent edges.

 

If you are unsure of what type of paper you are loading, such as bond or recycled paper, check the label on the package.

 

The following problems may cause print quality deviations, jamming, or even damage to the printer:

Paper Specifications

Folio

8.5 X 13 in.
(216 X 330 mm)

Minimum size (Custom)

3 x 5 in.
(76 x 127 mm)

60-210 g/m

2

bond (16-56 lb)

5 sheet of paper for the
multi-purpose feeder

Maximum size (Legal)

8.5 x 14 in.
(216 x 356 mm)

Transparency

Same minimum and
maximum paper sizes as
listed above.

138-146 g/m

2

(37-39 lb)

50 sheet of 75 g/m

2

bond

(20 lb) paper for the
multi-purpose feeder

Labels

120-176 g/m

2

(32-47 lb)

25 sheet of 75 g/m

2

bond

(20 lb) paper for the
multi-purpose feeder

Cards

60-210 g/m

2

(16-56 lb)

10 sheet of 75 g/m

2

bond

(20 lb) paper for the
multi-purpose feeder

Envelopes

75-105 g/m

2

(20-28 lb)

10 sheet of 75 g/m

2

bond

(20 lb) paper for the
multi-purpose feeder

NOTE:

You may experience jams when using print materials with a length of less than 127 mm (5 in). For optimum performance, ensure that you store

and handle the paper correctly. Please refer to

"Printer and Paper Storage Environment"

.

NOTE:

You can use A4, Letter, Folio, Oficio, Legal-sized paper for duplex printing.

Symptom

Problem with paper

Solution

Poor print quality or toner
adhesion, problems with feeding

Too moist, too rough, too smooth or
embossed; faulty paper lot

Try another kind of paper,
between 100-400 Sheffield, 4%-
5% moisture content.

Dropout, jamming, curl

Stored improperly

Store paper flat in its moisture-
proof wrapping.

Increased gray background
shading/printer wear

Too heavy

Use lighter paper, use the rear
door
.

Excessive curl problems with
feeding

Too moist, wrong grain direction or
short-grain construction

l

Use the rear door.

l

Use long-grain paper.

Jamming, damage to printer

Cutouts or perforations

Do not use paper with cutouts or
perforations.

Problems with feeding

Ragged edges

Use good quality paper.

NOTE:

Do not use letterhead paper printed with low-temperature inks, such as those used in some types of thermography.

NOTE:

Do not use raised or embossed letterhead.

NOTE:

The printer uses heat and pressure to fuse toner to the paper. Ensure that any colored paper or preprinted forms use inks that are compatible

with this fusing temperature (180° C or 356°

F for 0.1 second).

Category

Specifications

Acid Content

5.5 pH or lower

Caliper

0.094-0.18 mm (3.0-7.0 mils)

Curl in Ream

Flat within 0.02 in (5 mm)

Cut Edge Conditions Cut with sharp blades with no visible fray.

Fusing Compatibility Must not scorch, melt, offset, or release hazardous emissions when heated up to 180°

C (356°

F) for 0.1 second.

Grain

Long Grain

Moisture Content

4%-6% by weight