GC Kalore technical manual

Wear Test Results

Wear data was similar for both composite materials tested, despite the fact that the glass and
pre-polymerized filler particles in the KALORE without DuPont matrix were disrupted due to
shrinkage forces. This can be explained by the protective action of the innovative and newly
developed pre-polymerized fillers that are highly loaded with 400 nm glass filler and heat-cured.
the relatively high content of pre-polymerized fillers protects the resin effectively against three-
body wear.

4a. KALORE x2000 after 100,000 cycles.

note the continuous interface between the pre-polymerized fillers and the

resin matrix.

4b. KALORE without DuPont x2000 after 100,000 cycles.

note the gap at the interface between the pre-polymerized filler and the resin

matrix. Additionally, voids can be observed where fillers were lost.

4c. KALORE without DuPont x2000 after 100,000 cycles.

Note the loss of pre-polymerized fillers and glass particles from resin matrix.

Figure 4. SEM images of KALORE with

and without the DuPont matrix.