MECHANICAL

TEST ITEM

SPECIFICATION

Resistance to

There shall be

Temperature profile of reflow soldering

Soldering heat

no damage or

(reflow soldering)

problems.

The specimen shall be passed through the reflow oven with the

condition shown in the above profile for 1 time.

The specimen shall be stored at standard atmospheric conditions

for 1 hour, after which the measurement shall be made.

ELECTRICAL

TEST ITEM

SPECIFICATION

TEST DETAILS

Insulation

There shall be

DC 100V voltage shall be applied across this sample of top

resistance

no other

surface and the terminal.

damage or

The insulation resistance shall be more than 1

× 10

8

Ω.

problems.

Dielectric

There shall be

AC 100V voltage shall be applied for 1 minute acrosset the top

withstand

no other

surface and the terminal of this sample

voltage

damage or

problems.

Temperature

△L/L20℃≦

±10%

The test shall be performed after the sample has stabilized in

characteristics

0~2000 ppm/℃

an ambient temperature of -20 to +85℃,and the value

calculated based on the value applicable in a normal

temperature and narmal humidity shall be △L/L20℃≦

±10%.

Page-4/8

MSCDRI-104R-SERIES

Sodering temperature (

)

soldering
(Peak temperature 260±3℃ 10 sec

Slow cooling
(Stored at room
temperature)

30 sec Min

(230

+0

℃)

300
250

200

150

100

50

2 min

10
sec.

2 min. or more

Pre-heating

150 ~ 180℃

M A G . L A Y E R S