If the piece needs only shallow support of ¼” depth or

less, pour the alumina hydrate onto a ceramic fireclay shelf.

Support the fireclay shelf on three ½” posts to aid heat flow

under the shelf.

If the silver clay shape needs deeper support, pour the

alumina hydrate into an unglazed ceramic bisque bowl.

These are available at ceramic supply stores.

Place the ceramic bowl directly onto the kiln bottom.

NEVER use a glazed bowl to hold the alumina hydrate. If

the glaze runs, it can embed into the firing chamber.

Caution: Avoid breathing alumina hydrate dust.
Caution: Alumina hydrate can destroy the heating

element on contact. If it spills onto the firing cham-

ber, remove with a vacuum cleaner.

Venting the Kiln

Silver clay by itself needs no venting. Load the kiln, close

the door, and leave it closed until the clay silver is ready to re-

move.

The kiln needs venting if you fire ceramics or glass with

the clay silver, or if you make hollow objects that contain a

core of organic materials.

Paper maché and paper clay are good core materials. Do

not use wax or styrofoam as a core. They emit harmful

fumes.

Rate, Temperature, Hold

Each brand of silver clay fires to a specific temperature

and hold time. This information is available from your silver

clay supplier.

Note: Hold time is the length of time that the rec-

ommended temperature is maintained in the kiln.

Do not fire longer than the recommended hold, or

the silver will begin to overfire.

Besides selecting a temperature and hold time on your

kiln’s digital controller, you will also need a firing rate. (See

the separate digital controller instruction booklet.) Select a

Full Power rate if you are firing silver clay alone. If you fire

glass or ceramics with the silver clay, select a rate best suited

for the glass or ceramics.

Note: Do not place silver clay into a kiln that is al-

ready hot unless the clay is completely dry. The kiln

should be no hotter than 500°F/260°C when insert-

ing the silver clay.

After the kiln begins firing, leave the door closed. Do not

open the door until it is time to remove the clay. Visual in-

spection of the clay is unnecessary.

If you are firing glass with the silver clay, on the other

hand, you may need to check the fusing progress of the glass

by opening the door ½” and looking inside. Look for just a

second or two. As you gain experience, you will be able to

program the correct temperature for the silver clay and glass

combination, eliminating the need to visually check the

glass.

Cooling Time

After the clay silver has fired to completion, you can crack

the door an inch to speed cooling. If you are firing stones,

glass, or other materials with the silver clay, it is safer to allow

the kiln to cool slowly with door closed. Remove the piece

when the kiln reaches room temperature.

Silver clay pieces that contain no other materials can be

removed from the kiln at 1100°F/593°C. You can remove

them with tongs and drop them into water.

Caution: Turn the kiln off before inserting tongs

into the firing chamber. Wear protective gloves.

Combining Silver Clay

With Other Materials

There are two ways to fire silver clay with other materials

such as glass:

Fire the silver clay first by itself. After you have cleaned

and polished the silver clay, fire it a second time with the

other material.

Fire the silver clay and other materials, such as a stone,

together in a single firing.

Enameling powder is easier to fire with the silver clay in a

second firing. See page 12. Glass is often fired with the silver

clay in a single firing. Many types of glass will melt to the

point of overfire at silver clay temperatures. So before

combining glass and silver clay in a single firing, test a small

sample of the glass. To do this, fire the glass during a silver

clay firing, keeping the glass separate from the silver clay

piece. (This way you won’t ruin the silver clay piece.) Place

the glass pieces on a ceramic fireclay shelf. You must coat the

shelf with glass separator, or otherwise the glass sample with

embed into the shelf.

If the glass sample survives the firing, you can fire that

type of glass with silver clay in a single firing. Note, however,

that different types of glass fire to different temperatures.

Every time you fire a different type of glass, be sure to test.