25 . Re-open the on-off valve located near the filter and

allow the chemical to flow in an appropriate container .

If the chemical flow is unobstructed, the blockage

exists in the chemical hose which must be replaced .

26 . If the blockage persists, examine the tank filter . The

arrow on the filter should be pointing away from the

tank . If not, change the filter direction, steps 31-41 . If

the filter was installed correctly, continue with step 42 .

27 . Close the on-off valve .

28 . Close the chemical tank valve .

29 . Open the on-off valve located near the filter to

depressurize the filter .

30 . Disconnect the on-off valve from the filter .

31 . Disconnect the filter from the chemical tank valve .

32 . Reconnect the new filter with the arrow pointing away

from the tank .

33 . Reconnect the on-off valve with the swivel to the filter .

34 . Tighten all connections with an adjustable wrench .

35 . Verify that the on-off valve is closed . The handle should be

perpendicular to the valve .

36 . Open the chemical tank valve .

37 . Open the on-off valve and allow the chemical to

flow in an appropriate container . If the flow is full,

reconnect the chemical hose and Gun/Hose assembly

and perform steps 16-23 . If the flow is weak the problem

exists in the tank . Contact your Dow Sales Representative

for assistance .

Section 11

Yield Notes

Board foot yields are based on the free rise of the total weight of
the chemicals in the tanks . Many factors affect the yield in field
applications .

11 .1 Operator Technique

For best results, apply multiple layers of foam . When spraying,
apply one-quarter to one-half inch thickness of uncured foam .

This will produce a one to one-and-one-half inch thickness of

fully cured foam .

11 .2 Application

avoid spraying over rising foam .

11 .3 Temperature

To ensure proper chemical mix, reaction, cure, and optimum

yields, chemicals should not be dispensed if the chemical
temperature is below 65°F (18°C) . Insufficient operating
temperatures can cause improper mix, extend cure time, and
adversely affect final physical properties and yields .

nOTe: When using polyurethane foam, estimate 30% more foam than is

required. This yield buffer is recommended so that you will not run out of

chemical on a job site.