E-3

TROUbLESHOOTING

E-3

Observe all Safety Guidelines detailed throughout this manual

PRObLEMS

(SYMPTOMS)

POSSIbLE

CAUSE

RECOMMENDED

COURSE OF ACTION

Oxidation

Tungsten inclusions

Porosity

Hot cracking

1. lnsufficient gas.
2. No protection on the back side.

1. lncorrect electrode sharpening.
2. Electrode too small.
3. Operating failure (contact of the

tip with the workpiece).

1. Dirt on the edges.
2. Dirt on the filler material.
3. Excessive travel speed.
4. Current intensity too low.

1 Unsuitable filler material.
2. High heat supply.
3. Dirty materials.

If all recommended possible areas of
misadjustment have been checked
and the problem persists, Contact
your local Lincoln Authorized
Field Service Facility.