Surface Mount Information

(continued)

Lead Free Soldering

The –Z version Austin SuperLynx SMT modules are
lead-free (Pb-free) and RoHS compliant and are both
forward and backward compatible in a Pb-free and a
SnPb soldering process. Failure to observe the
instructions below may result in the failure of or cause
damage to the modules and can adversely affect
long-term reliability.

Pb-free Reflow Profile

Power Systems will comply with J-STD-020 Rev. C
(Moisture/Reflow Sensitivity Classification for
Nonhermetic Solid State Surface Mount Devices)
for both Pb-free solder profiles and MSL
classification procedures. This standard provides a
recommended forced-air-convection reflow profile
based on the volume and thickness of the package
(table 4-2). The suggested Pb-free solder paste is
Sn/Ag/Cu (SAC). The recommended linear reflow
profile using Sn/Ag/Cu solder is shown in Fig. 37.

MSL Rating

The

Austin SuperLynx SMT modules have a MSL

rating of 2a.

Storage and Handling

The recommended storage environment and
handling procedures for moisture-sensitive surface
mount packages is detailed in J-STD-033 Rev. A
(Handling, Packing, Shipping and Use of
Moisture/Reflow Sensitive Surface Mount Devices).
Moisture barrier bags (MBB) with desiccant are
required for MSL ratings of 2 or greater. These

sealed packages should not be broken until time of
use. Once the original package is broken, the floor
life of the product at conditions of

≤ 30°C and 60%

relative humidity varies according to the MSL rating
(see J-STD-033A). The shelf life for dry packed
SMT packages will be a minimum of 12 months
from the bag seal date, when stored at the
following conditions: < 40° C, < 90% relative
humidity.

Post Solder Cleaning and Drying
Considerations

Post solder cleaning is usually the final circuit-board
assembly process prior to electrical board testing. The
result of inadequate cleaning and drying can affect
both the reliability of a power module and the
testability of the finished circuit-board assembly. For
guidance on appropriate soldering, cleaning and
drying procedures, refer to Board Mounted Power
Modules: Soldering and Cleaning
Application Note
(AN04-001).

Per J-STD-020 Rev. C

0

50

100

150

200

250

300

Reflow Time (Seconds)

R

efl

ow

T

em

p

C

)

Heating Zone
1°C/Second

Peak Temp 260°C

* Min. Time Above 235°C
15 Seconds

*Time Above 217°C

60 Seconds

Cooling
Zone

Figure 37. Recommended linear reflow profile
using Sn/Ag/Cu solder.