Machining strategies

Top and bottom surface are often different, hole quality

can therefore depend on where the drill enters or exits.

A coating or surface layer on the carbon fibre can

change the output completely.

For example:

-

Lightning Strike Protection (LSP): a fine or coarse copper mesh, allows for

higher feed rate

-

Glass-cloth coating: increases the risk of delamination

-

Both materials can be more easily machined by chosing the correct geometry.

CoroDrill 854

CoroDrill 856

Delamination

Lightning Strike Protection (LSP) layer on
CFRP material

CFRP with glass-cloth coating

Solution

Splintering/ fraying

Hole quality issue

CoroDrill 854: Point geometry designed to prevent
splintering and fraying.

CoroDrill 856: Designed to reduce delamination
problems.