DANGER! Ensure that the machine is disconnected from the power supply before performing service or

maintenance on any part of the unit, cables or torch.

7.1.

The inverter

DO NOT open the unit. Service and maintenance of the machine must only be undertaken by an

authorised service agent.

7.1.1.

Keep the machine clean by wiping with a soft cloth. Do not use abrasives.

7.1.2.

Periodically check to ensure that the carrying handle is in good order and condition. If not replace it

immediately.

7.1.3.

Ensure that the front and rear air vents are not blocked.

7.2.

Cables and leads

7.2.1.

Check to ensure cables and leads are in good condition. If damaged, contact your authorised service

agent.

7.2.2.

Keep cables and leads clean. Do not use solvents.

7.3. Torch

Check torch regularly. Maintenance will depend on frequency and type of usage and is essential for correct

and safe use of the torch.

WARNING! Ensure that the torch is cool before attempting any maintenance. Always re-assemble the torch

in the correct order as shown in (fig.9). Never use tools to tighten nozzle components, hand tighten only.

Manually dismantle the torch nozzle head.

7.3.1.

Cap (fig.9.1).

Clean cap and check to ensure it is not damaged (including distortion, burns, cracks). If in any doubt,

replace.

7.3.2.

Electrode

(fig.9.2).

Check the build-up on the emitting surface of the electrode. When the build-up is approximately 2mm

replace the electrode.

NOTE: We recommend that the electrode and nozzle are changed at the same time.

7.3.3.

Air distribution ring (fig.9.3).

Check that the ring is not burned or cracked and that the airflow holes are not obstructed. If damaged,

replace.

7.3.4.

Nozzle (fig.9.4).

If the surface is oxidised, clean with extra fine abrasive paper. Check wear of the plasma arc hole and the

inner and outer surfaces. If hole has widened, or nozzle is damaged in any way, replace it. The nozzle “V”

crater should be 1.5mm in depth (fig.10).

7. MAINTENANCE

fig.10

8. TROUBLESHOOTING

9. RATING PLATE

fig.9

PROBLEM

POSSIBLE CAUSE

REMEDY

Insufficient penetration or excessive scoria settlement.

Cutting speed too fast.

Torch angle too great.

Workpiece is too thick.

Electrode and nozzle are worn out.

Slow the cutting speed.

Adjust the torch angle.

Confirm workpiece thickness and re-check technical data.

Replace electrode and nozzle.

Interruption of cutting arc.

Cutting speed too low.

Excessive distance between torch and workpiece.

Electrode is worn out.

Intervention of the protection system.

Increase the cutting speed.

Decrease the distance between torch and workpiece.

Replace electrode and nozzle.

Check warning lights and take appropriate action.

The torch is cutting at tilt when you wish it to be

perpendicular.

Torch position not correct.

Asymmetric wear of nozzle hole and/or wrong assembly of

torch parts.

Re-align the torch.

Check assembly (see fig.5) and change nozzle if necessary.

Excessive wear of nozzle and electrode.

Air pressure too low.

Contaminated air (humidity-oil).

Excessive pilot arc ignitions in the air.

Nozzle holder damaged.

Increase air pressure (see Section 5).

Check air supply system (see Sections 4, 5 & 7).

Do not casually turn the torch on and off.

Change the nozzle holder.

Original Language Version

PP40H Issue: 1 - 08/05/13

Equipment safety standard

Internal wiring information

Plasma symbol

AC supply details

Insulation protection rating

Max open circuit voltage

Rated supply voltage

Max RMS current absorbed

Effective current supplied

X Duty cycle based on 10 mins (35%

indicates 3.5mins cutting 6.5mins rest,

100% indicates continuous usage.

I

2

, U

2:

current and corresponding

voltage.

SERIAL NUMBER

PP40H

Cutting current range and

corresponding voltages.

Unique number