Welding Power Source Duty Cycle And Overheating

Duty Cycle is percentage of 10 min-
utes that unit can weld at rated load
without overheating.

If unit overheats, thermostat(s)
opens, output stops, and cooling
fan runs. Wait fifteen minutes for
unit to cool. Reduce amperage or
duty cycle before welding.

Y

Exceeding duty cycle can
damage unit or gun and void
warranty.

30% Duty Cycle At 130 Amperes

Overheating

0

15

A or V

OR

Reduce Duty Cycle

Minutes

duty1 4/95 – SB-180 844

300

250

200

150

100

75

50

10

15

20

25 30

40

50 60 70 80 100

DC AMPERES

% DUTY CYCLE

3 Minutes Welding

7 Minutes Resting

2-4.

Welding Gun Duty Cycle And Overheating

CAUTION

WELDING LONGER THAN RATED DUTY CYCLE can damage gun and void warranty.

Do not weld at rated load longer than shown below.

Using gasless flux cored wire reduces gun duty cycle.

warn7.1 8/93

Duty Cycle is percentage of 10
minutes that gun can weld at
rated load without overheating.

Continuous Welding

SB1.1 8/93

0

10

Minutes

Definition

.023 To .045 in (0.6 To 1.1 mm)

Hard Or Flux Cored Wires

100% Duty Cycle At 100 Amperes

Using CO

2

.023 To .045 in (0.6 To 1.1 mm) Hard Or Flux Cored Wires

60% Duty Cycle At 100 Amperes

Using Mixed Gases

6 Minutes Welding