Weldskill 100 inverter, 11 joint preparations – Tweco 100 Weldskill User Manual

Page 27

Advertising
background image

weldskill 100 iNVeRTeR

4-5

March 3, 2008

4.11 Joint Preparations

In many cases, it will be possible to weld steel sections without any special preparation. For heavier sections

and for repair work on castings, etc., it will be necessary to cut or grind an angle between the pieces being

joined to ensure proper penetration of the weld metal and to produce sound joints.
In general, surfaces being welded should be clean and free of rust, scale, dirt, grease, etc. Slag should be

removed from oxy-cut surfaces. Typical joint designs are shown in Figure 4-10.

Gap varies from 1.6mm to 4.8mm depending

on plate thickness

Joint

Open Square Butt

1.6mm max

1.6mm

Single Vee Butt Joint

Not less than

70°

Double Vee Butt Joint

1.6mm

Lap Joint

Tee Joints

(Fillet both sides of the

joint)

Edge Joint

Fillet Joint

Corner Weld

Plug Weld

Plug Weld

Not less than

70°

Single Vee Butt Joint

Not less than

45°

1.6mm max

Art # A-07695

Figure 4-10: Typical joint designs for arc welding