7-9. Lap Joints

S-0063 / S-0064

1

Electrode

2

Single-Layer Fillet Weld

Move electrode in circular motion.
3

Multi-Layer Fillet Weld

Weld a second layer when a larger

fillet is needed. Remove slag before

making another weld pass. Weld

both sides of joint for maximum

strength.

30

°

Or Less

Single-Layer Fillet Weld

Multi-Layer Fillet Weld

30

°

Or Less

1

1

2

3

7-10. Tee Joints

S-0069 / S-0058-A / S-0061

1

Electrode

2

Fillet Weld

Keep arc short and move at definite

rate of speed. Hold electrode as

shown to provide fusion into the

corner. Square edge of the weld

surface.
For maximum strength weld both

sides of upright section.
3

Multi-Layer Deposits

Weld a second layer or more when

a larger fillet is needed. Use any of

the weaving patterns shown in Sec-

tion 7-7. Remove slag before mak-

ing another weld pass.

45

°

Or Less

1

2

2

1

3

7-11. Welding Troubleshooting

Table 6-1. Porosity

Porosity − small cavities or holes resulting

from gas pockets in weld metal.

Possible Causes

Corrective Actions

Arc length too long.

Reduce arc length.

Damp electrode.

Use dry electrode.

Workpiece dirty.

Remove all grease, oil, moisture, rust, paint, coatings, slag, and dirt from work surface before

welding.