3. welding gun duty cycle and overheating, 4. volt-ampere curves, Caution – Hobart Welding Products IRONMAN M-10 User Manual

Page 14

Advertising
background image

OM-927 Page 10

3-3. Welding Gun Duty Cycle And Overheating

CAUTION

WELDING LONGER THAN RATED DUTY CYCLE can damage gun and void warranty.

Do not weld at rated load longer than shown below.

Using gasless flux cored wire reduces gun duty cycle.

warn7.1 8/93

Duty Cycle is percentage of 10

minutes that gun can weld at

rated load without overheating.

Continuous Welding

SB1.1 8/93

0

10

Minutes

Definition

.023 To .045 in (0.6 To 1.1 mm)

Hard Or Flux Cored Wires

100% Duty Cycle At 100 Amperes

Using CO

2

.023 To .045 in (0.6 To 1.1 mm) Hard Or Flux Cored Wires

60% Duty Cycle At 100 Amperes

Using Mixed Gases

6 Minutes Welding

4 Minutes Resting

3-4. Volt-Ampere Curves

Volt-ampere curves show minimum

and maximum voltage and amper-

age output capabilities of unit.

Curves of other settings fall be-

tween curves shown.

va_curve1 4/95 − 199 212

0

5

10

15

20

25

30

35

0

50

100

150

200

250

DC AMPERES

DC VOL

TS