Solvent

Resistance

Acetaldehyde

B

Acetone

A

Benzene

A

Butanol

A

Chloroform

A

Diethyl ether

A

Dimethylformamide

A

Dimethylbenzene (Xylol)

A

Dioxane

A

Acetic acid

A

Acetic acid anhydride

A

Ethanol

A

Ethyl acetate

A

Hexane

A

Isobutanol

A

Isopropanol

A

Methanol

A

Methylene chloride

A

Nitrobenzene

A

Phenol

A

Propanol

A

Sulphuric acid, fuming

A

Carbon tetrachloride

B

Tetrahydrofurane

A

Tolene

A

Triethylamine

A

Trichloroacetic acid

A

Trichloroethane

A

Trifluoroacetic acid

A

Vinylidene chloride (Dichloroethylene)

A

Aqueous hydrogen bromide, saturated

A

Aqueous hydrogen chloride, saturated

A

Aqueous ammonia solution

A

Aqueous caustic soda

A

Aqueous nitric acid

A

Table 9: Resistance of the perfluorelastomer sealings

Resistance of the perfluorelastomer sealings

A: Very good resistance: Perfluorelastomer may be used

without restrictions

B: Moderate resistance: Sealing made of Perfluorelastomer

may swell. Sealings may generally be used, but may
under some circumstances have to be replaced after
being used several times.

C: Poor resistance: Sealing deform. The sealings of Per-

fluorelastomer should be used only to a limited extent.
We recommend that the sealings be tested beforehand
(softening or wetting the sealing discs).

D: Very poor resistance: Sealing deform. The sealing of

Perfluorelastomer should not be used.