– Mix the Polymer and Monomer Modifier in a 1.3 : 1

ratio and leave to rest uncovered for 2–3 minutes.

– Polymerization is conducted in a pressure device or in

a heat/pressure polymerization unit (eg Ivomat),
15 minutes at 40–50 °C / 104–122 °F and 2–6 bar
pressure.

If necessary, radiographic balls or similar aids may be
integrated into the diagnostic stents where they are
needed.

Mix the Monomer and Polymer Modifier

Secure the key

Pour the liquid material into the key

After polymerization