Ironwood Electronics Solder Column Interface Soldering Techniques User Manual

Page 2

Advertising
background image

Page 2 of 2

Solder Column Interface Soldering Techniques (continued)

Tel: (800) 404-0204

www.ironwoodelectronics.com

See manufacturer’s recommendation for your specific application.

(6) Clean PCB with the flux manufacturers recommended process. The picture of the solder
connection is shown in Figures 4 and 5.

250

200

150

100

50

0

100

200

300

400

500

Preheat

Flux Activation

Reflow

Cool-Down

<2°C
per Second

150 - 180 Seconds

<2°C

per Second

1° to 3°C
per Second

Time (seconds)

Temperature

(°C)

Maximum Package Body Temperature

Solder Temperature Melting Point

Example 63/37 Reflow Profile

Figure 4: Magnified View of Solder
Connections

Figure 5: Solder Connections

Advertising