After staining, the stain and characterization firing is conducted in a compatible ceramic furnace (e.g. P500). The following

points should be observed when placing the restoration in the furnace and setting the firing parameters:

– Place veneers as well as anterior and posterior crowns on metal pins and position them on the honey-comb firing tray.

– To better secure the restoration on the metal pins (particularly with veneers), a small amount IPS Object Fix may also be

used.

IPS Empress CAD with IPS Empress Universal

B

S

t

T H

V

1

V

2

Stain and Characterization firing

403°C

6'

100°C

790°C

1'

450°C

789°C

757°F

6'

180°F

1454°F

1'

842°F

1453°F

Firing parameters for the Stain and Characterization firing

(note the temperature control)

Place the objects on the honey-comb firing tray and start the firing program

Optional

Shade check

To check the tooth shade after the first stain and characterization firing,

proceed as follows:

– Wet inner aspects of the restoration with IPS Contour Glaze and Stain

Liquid using a brush.

– Place the restoration on the individual control die and check the tooth

shade, as well as the individualized effects.

– If adjustments are required, apply the corresponding stains and fire

them using the above firing program.

Shade check. If necessary, the shade intensity can be increased

by additional staining.