Arcmaster 300 acdc – Tweco 300 DC Arcmaster User Manual

Page 55

Advertising
background image

ARCMASTER 300 ACDC

February 22, 2006

10-5

A Small electrodes used on

heavy cold plate.

A Use larger electrodes and

pre-heat the plate.

B Welding current is too low.

B Increase welding current.

C Wrong electrode angle.

C Adjust angle so the welding

arc is directed more into the
base metal.

D Travel speed of electrode is

too high.

D Reduce travel speed of

electrode.

E Scale or dirt on joint

surface.

E Clean surface before

welding.

Remedy

4 Portions of the weld

run do not fuse to the
surface of the metal or
edge of the joint.

Description

Possible Cause

Table 10-2 (continued): Stick Welding Problems

Lack of fusion caused by dirt,
electrode angle incorrect,
rate of travel too high

Lack of side fusion, scale
dirt, small electrode,
amperage too low

Lack of inter-run
fusion

Lack of root fusion

Art # A-04992

Figure 10-2: Example of lack of fusion