Parting – thin-walled tubes

When parting off into thin-walled tubes ensure the lowest possible cutting forces are gener-
ated. Use inserts with smallest possible width and sharpest edges, i.e. CF or CS geometries.
The precision ground CoroCut XS in combination with widths down to 0.7 mm gives the
lowest cutting forces.