Symptom

Problem with

paper

Solution

Poor print quality or toner

adhesion, problems with feeding

Too moist, too

rough, too smooth or
embossed; faulty paper lot

Try another kind of

paper, between 100-400
Sheffield, 4%-5%
moisture content.

Dropout, jamming, curl

Stored improperly

Store paper flat in

its moisture-proof
wrapping.

Increased gray background

shading/printer wear

Too heavy

Use lighter paper,

use the rear door.

Excessive curl problems with

feeding

Too moist, wrong

grain direction or short-
grain construction

Use the rear

door.

Use long-grain

paper.

Jamming, damage to printer

Cutouts or

perforations

Do not use paper

with cutouts or
perforations.

Problems with feeding

Ragged edges

Use good quality

paper.

NOTE:

Do not use letterhead paper printed with low-temperature inks, such as those used in some

types of thermography.

NOTE:

Do not use raised or embossed letterhead.

NOTE:

The printer uses heat and pressure to fuse toner to the paper. Insure that any colored paper or

preprinted forms use inks that are compatible with this fusing temperature (180° C or 356° F for 0.1
second).

Paper Specifications

Category

Specifications

Acid Content

5.5 pH or lower

Caliper

0.094-0.18 mm (3.0-7.0 mils)

Curl in Ream

Flat within 0.02 in. (5 mm)

Cut Edge Conditions

Cut with sharp blades with no visible fray.

Fusing Compatibility

Must not scorch, melt, offset or release hazardous

emissions when heated to 180° C (356° F) for 0.1 second.

Grain

Long Grain

Moisture Content

4%-6% by weight

Smoothness

100-400 Sheffield