Emissivity table (continue)
Material
Temperature(°C)
Emissivity
approximation
Lead
Pure lead (Non-
oxidization)
125~225
0.06~0.08
Mildly oxidized
25~300
0.20~0.45
Magnesium
Magnesia
275~825
0.55~0.20
Magnesia
900~1670
0.20
Hg
0~100
0.09~0.12
Nickel
Electroplate polishing 25
0.05
Electroplate
20
0.01
non-polishing
Nickel wire
185~1010
0.09~0.19
Nickel plate (oxidized) 198~600
0.37~0.48
Nickel oxide
650~1255
0.59~0.86
Nickel alloy
Nickel-chrome (heat-
resistance) alloy wire
(shining)
50~1000
0.65~0.79
Nickel-chrome alloy
50~1040
0.64~0.76
Nickel-chrome (heat
resistance)
50~500
0.95~0.98
Nickel-silver alloy
100
0.14
Silver
Polished silver
100
0.05
Advertising