15

Engine/Cylinder Head, Valves

944

Remachining cylinder-head maling face

Checking cylinder head for distortion

Use a feeler gage an a straight edge or a

precision straight edge to check the maling

face of the cylinder head for distortion.

Permissible maling-face uneveness: 0.05

mm

Cylinder heads with distorted maling faces

can be remachined and reused. Permissible

rough atter finishing: 0.03 mm.

Remachining cylinder head

Do not remove mor material from the cylinder

head maling face than is necessary to

achieve a smooth surface. Max. machining

depth 146.6 mm.

Note on machining maling face:

Peak-to-valley = 0.015 mm

If the new-dimension tolerance is exceeded

during machining, a cylinder head gasket

with a thickness of 1.4 mm must be fitted.

Size new

Size worn

= 147 +- 0.1 mm

= 146.6 mm

1126-15

Cylinder head refacing dimension and

identification

New dimension

Gasket

Identification

Refacing dimension

Gasket

Identification

: 147 +- 0.1 mm

: 1.1 mm

: none

: 146.8 to 146.6 mm

: 1.4 mm

: N

Identification "N"

To be embossed on exhaust side, between

cylinders no. 2 and 3, on the casting lug

below

the sealing face of the cylinder head cover.

Punch character height "N" = 6 mm

15 - 120