4.07 Cut Quality

Cut quality requirements differ depending on application. For instance, nitride build-up and bevel angle may be

major factors when the surface will be welded after cutting. Dross-free cutting is important when finish cut quality

is desired to avoid a secondary cleaning operation. Cut quality will vary on different materials and thicknesses.

Right Side

Cut Angle

Left Side

Cut Angle

A-00512

Kerf Width

Cut Surface

Bevel Angle

Top Edge

Rounding

Cut Surface

Drag Lines

Dross

Build-Up

Top

Spatter

A-00007

Cut Surface

The condition (smooth or rough) of the face of the cut.

Bevel Angle

4. Place the RUN/SET switch to the RUN position.

The angle between the surface of the cut edge and a plane perpendicular to the surface of the plate. A perfectly

perpendicular cut would result in a 0° bevel angle.

Top-Edge Rounding

Rounding on the top edge of a cut due to wearing from the initial contact of the plasma arc on the workpiece.