Fabricator 141i

BASIC WELDING GUIDE

4-16

Manual 0-5145

Art # A-07700_AB

1

2

3

4

5

6

Figure 4-24: Multi-runs in HV Fillet Weld

C. Vertical Welds

1. Vertical Up

Tack weld a three feet length of angle iron to your work bench in an upright position. Use a 1/8"(3.2mm)

E7014 Stick electrode and set the current at 100 amps. Make yourself comfortable on a seat in front of the

job and strike the arc in the corner of the fillet. The electrode needs to be about 10º from the horizontal to

enable a good bead to be deposited. Refer Figure 4-25. Use a short arc, and do not attempt to weave on

the first run. When the first run has been completed de-slag the weld deposit and begin the second run at

the bottom. This time a slight weaving motion is necessary to cover the first run and obtain good fusion

at the edges. At the completion of each side motion, pause for a moment to allow weld metal to build up

at the edges, otherwise undercut will form and too much metal will accumulate in the centre of the weld.

Figure 4-26 illustrates multi-run technique and Figure 4-27 shows the effects of pausing at the edge of

weave and of weaving too rapidly.

Art # A-07701

Figure 4-25: Single Run Vertical Fillet Weld

Art # A-07702

Figure 4-26: Multi Run Vertical Fillet Weld