Note

Observe the curing depths of the materials. Depending on the layering technique, more or less air is
trapped in the veneering material. This may lead to porosity and, in extreme cases, slightly influence the
shade. In order to prevent this situation, the restoration can be compressed in the Ivomat for 2 minutes
at 6 bar/87 psi (without heat and without water) immediately after contouring. Poylmerization with
light is carried out immediately after that.

Polymerization

– Remove the completely layered restoration from the model and supplement the contact points with

Telio Lab LC Incisal materials, if required. Make sure that good adaptation in the marginal areas is
achieved, i.e. at the transtion between Telio Lab / Talio CAD and the veneer.

– Coat the completely contoured veneer with a generous amount of SR Gel and polymerize.
– After polymerization, thoroughly remove the SR Gel under running water.

36

The respective light-curing Telio components are pre-polymerized to ensure that they stay in place and to
be able to apply a further layer. However, final polymerization of the entire restoration is always required.

Polymerization device

Manufacturer

Pre-polymerization

Polymerization

Quick

Ivoclar Vivadent

40 s (SR Composiv 60 s)

––

Lumamat

®

100 (Targis

®

Power

Upgrade)

Ivoclar Vivadent

Exclusively use Quick for pre-polymerization.

11 min
(program P 2)

Spectramat

®

Ivoclar Vivadent

5 min (Telio Stains 2.5 min)

5 min