Crystallization and Stain/Glaze Firing
Basically, fully anatomically milled restorations made of IPS e.max CAD can be completed in three different ways.
IPS e.max CAD LT crown on the model
IPS e.max CAD HT inlay/onlay on the model.
Option A:
Crystallization and Glaze firing with
IPS e.max CAD Crystall./Glaze paste
Option B:
Crystallization and Stain/Glaze firing
with IPS e.max CAD Crystall./Glaze spray
Option C:
Crystallization and separate Stain/Glaze
firing with IPS e.max Ceram Shades,
Essences and Glaze
Characterization of the non-crystallized,
blue restoration permits quick comple-
tion of the restoration with the
subsequent combination firing
(Crystallization/Glaze HT/LT).
Characterization of the non-crystallized,
blue restoration permits quick comple-
tion of the restoration with the
subsequent combination firing
(Crystallization/Glaze HT/LT).
Characterization of the tooth-coloured
restoration after crystallization.