– Crystallization/Glaze HT/LT can only be used for IPS e.max CAD HT and LT.

– IPS e.max CAD MO cannot be crystallized with this program, since it does not crystallize

completely.

– If only max. two restorations are crystallized at the same time, the closing time S can be

reduced to 1:30 min. This reduced time is only for Glaze Spray. Glaze Paste may not be

used.

Furnace

P100
P200

P300
P500
P700

PX1

EP 600

EP 3000
EP 5000

Closing time

S

min.

6:00

6:00

6:00

6:00

6:00

Stand-by

temperature

B

°C/°F

403/757

403/757

403/757

403/757

403/757

Heating rate

t

1

°C/°F/min

90/162

90/162

90/162

90/162

90/162

Firing

temperature

T

1

°C/°F

820/1508

820/1508

820/1508

820/1508

820/1508

Holding time

H

1

min.

0:10

0:10

0:10

0:10

0:10

Heating rate

t

2

°C/°F/min

30/54

30/54

30/54

30/54

30/54

Firing

temperature

T

2

°C/°F

840/1544

840/1544

840/1544

840/1544

840/1544

Holding time

H

2

min.

7:00

7:00

7:00

7:00

7:00

Long-term

cooling

L

°C/°F

700/1292

700/1292

775/1427

1:30 min

700/1292

0:20 min

700/1292

700/1292

Cooling rate

t

l

°C/°F/min

0

0

Vacuum 1

1

1

1

2

°C/°F

550/1022
820/1508

550/1022
820/1508

550/1022
820/1508

550/1022
820/1508

550/1022
820/1508

Vacuum 2

2

1

2

2

°C/°F

820/1508
840/1544

820/1508
840/1544

820/1508
840/1544

820/1508
840/1544

820/1508
840/1544

Crystallization/Glaze HT/LT

IPS e.max CAD HT/LT with or without application of IPS e.max CAD Crystall./Glaze, Shades, Stains, and Add-On

Correction firing

with IPS e.max CAD Crystall./Glaze, Shades, Stains, or Add-On

Only the program memories 65-69 can be used with the Programat P100.

Furnace

P80

P100
P200

P300
P500
P700

PX1

EP 600

EP 3000
EP 5000

Closing time

S

min.

6:00

6:00

6:00

6:00

6:00

6:00

Stand-by

temperature

B

°C/°F

403/757

403/757

403/757

403/757

403/757

403/757

Heating rate

t

1

°C/°F/min.

90/162

90/162

90/162

90/162

90/162

Firing

temperature

T

1

°C/°F

820/1508

820/1508

820/1508

820/1508

820/1508

Holding time

H

1

min.

0:10

0:10

0:10

0:10

0:10

Heating rate

t

2

°C/°F/min

30/54

30/54

30/54

30/54

30/54

30/54

Firing

temperature

T

2

°C/°F

840/1544

840/1544

840/1544

840/1544

840/1544

840/1544

Holding time

H

2

min.

3:00

3:00

3:00

3:00

3:00

3:00

Long-term

cooling

L

°C/°F

700/1292

700/1292

700/1292

775/1427

1:30 min

700/1292

0:20 min

700/1292

700/1292

Cooling rate

t

l

°C/°F/min

0

0

Vacuum 1

1

1

1

2

°C/°F

550/1022
820/1508

550/1022
820/1508

550/1022
820/1508

550/1022
820/1508

550/1022
820/1508

Vacuum 2

2

1

2

2

°C/°F

550/1022
840/1544

820/1508
840/1544

820/1508
840/1544

820/1508
840/1544

820/1508
840/1544

820/1508
840/1544

Only the program memories 65-69 can be used with the Programat P100.