OPERATION

B-19

B-19

VRTEX

TM

360

Travel Speed

is how fast the electrode is traveling in

respect to the workpiece.

Dime Spacing

is the distance from one solidified weld

puddle to the next. (whip technique only)

Whip Time

is the time the user is in the whipping

motion, or not dwelling in the weld puddle. (whip tech-

nique only)

Dwell Time

is the time the user is dwelling, or keeping

the VR Stick electrode in the virtual puddle. (whip

technique only)

Width of Weave

is the side-to-side distance of where

the VR GMAW/FCAW gun or VR SMAW device was

aimed when completing one weave cycle in a series

that make up a weld.

Weave Timing

is the time taken to complete one side

to side weaving motion.

Weave Spacing

is the distance in the overall direction

of travel between one weave cycle in a series that

make up a weld.

Pass number

The pass number is displayed on the left center of the

screen. To change the pass being viewed, use the joy-

stick to highlight the pass number and then joystick left

or right to change the pass number. For pipe, the infor-

mation is displayed in a similar manner on a 2D screen

as though the pipe is unraveled and put on a flat sur-

face. The user can choose between viewing the whole

pipe or one of the four quadrants of the pipe. Use the

joystick to highlight the pipe section desired.

Travel Direction

The travel direction is located on the right side in the

middle of the screen. When the user first starts to

weld, a travel direction is sensed by the system and an

arrow indicating the direction is displayed. For visual

cues, the system assumes these directions. The visu-

al cues will automatically adapt to the travel direction

used when the arc is struck.

Bead Render

An image of the completed pass appears in the middle

of the screen.

Discontinuity Indicator

The lower left side of the screen list potential disconti-

nuities. When a student uses incorrect welding tech-

niques, this causes specific weld discontinuities. A line

is drawn at the location indicating these discontinuities.

For example, too long an arc length will cause porosi-

ty.

Potential discontinuities include:

• Incomplete Fusion/Penetration

• Slag Inclusion

• Porosity

• Undercut

• Poor Bead Placement

• Wrong Weld Size

• Convex/Excessive Reinforcement

• Concave/Underfill

• Excess Spatter

• Melt Through/Blow Through

Return

to

Section

TOC

Return

to

Section

TOC

Return

to

Section

TOC

Return

to

Section

TOC

Return

to

Master

TOC

Return

to

Master

TOC

Return

to

Master

TOC

Return

to

Master

TOC

Advertising