Stainless steel, Above water only, 40 amps • air plasma / air shield – Hypertherm HT2000-200 Volt User Manual

Page 122

Advertising
background image

HySpeed HT2000

Instruction Manual

6-27

OPERATION

22

Shield

Arc

Approx.

Material

Plasma Gas Flow Rate %

Gas (Air)

Torch-to-work

Initial Torch

Voltage

Motion

Thickness

Preflow

Cutflow

Pressure

Distance

Piercing Height

Setting

Travel Speed

Delay Time

(inches)

(mm)

(Air %)

(Air %)

(psi)

(inches)

(mm)

(inches)

(mm)

(volts)

(ipm) (mm/min.)

(sec)

.050

(18 GA.)

40

20

60

3/32

2.5

3/16

5

120

145

3700

1/16

1.5

(46.0

(23.1

(275

3/32

2.5

3/16

5

120

120

3050

1/8

3

SCFH)

SCFH)

SCFH)

3/32

2.5

3/16

5

125

75

1900

0.5

1/4

6

1/8

3

135

24

610

3/8

10

1/8

3

140

12

300

Stainless Steel

40 amps • Air Plasma / Air Shield

This gas combination gives good cut speed, low dross level and is very economical. Some surface nitriding and

surface oxidation of alloying elements can occur.

Notes:

Set air plasma gas inlet pressure to 90 psi (6.2 bar)
Set air shield gas inlet pressure to 90 psi (6.2 bar)
Production cutting above 1/8" (3 mm) not recommended

Above Water Only

020688
Shield

020423
Retaining cap

020689
Nozzle

020613
Swirl ring

120667
Electrode